Recap: Capital Region BOCES Industry Advisory Meeting and Lincoln Hyperfill Demo

Date of Event: 12/18/2024

Location: Capital Region BOCES CTE, Albany, N.Y

Number of Attendees: 26

Presenter/Notable Guest(s): Padraic Bean, Lincoln Electric
Sam DiPasquale, Lincoln Electric
Chris Johnson, Instructor Capital Region BOCES
Micah Belgiano, Instructor Capital Region BOCES
Don Mattoon, Instructor Capital Region BOCES 

Event Summary: Section members participated in an evening of welding and camaraderie at Capital Region BOCES for their annual advisory board meeting. During this meeting section members were able to connect with industry professionals, share insights, and contribute to the future of education and workforce development. In addition to the Advisory Meeting, Lincoln Electric was on sight demonstrating their high deposition twin wire Hyperfill technology.