October 21, 2021 – Tennessee Central Railway Museum; Nashville, TN
Thanks to Stephen Hook and John Hayes for a review of their experience obtaining and working with the materials of construction used during the ongoing Steam Locomotive 576 preservation project, and joining methods used. Joining methods discussed included not only welding but riveting also. This was the Nashville Sections first attempt at a hybrid event using the Meeting Owl. Thanks to all virtual attendees for their patience!
Stephen Hook rivets the firebox of the Nashville Steam Preservation Society Steam Locomotive 576