Month: April 2026

Guest Speaker: Michael J. O’Connor – Executive Director, The Connecticut Port Authority

Join us on Wednesday, May 13 at 5:30PM EST to hear from Michael J. O’Connor, Executive Director, The Connecticut Port Authority.  The Connecticut Port Authority was established in 2014, and its mission is to grow Connecticut’s economy by strategically investing in the state’s three deep-water ports and small harbors to enable each to maximize its own economic potential.…

Recap: Tour of Lynn Welding’s Resistance Welding Department

Date of Event: 04/14/2026 Location: 75 Rockwell Street, Newington, CT Number of Attendees: 10 Presenter/Notable Guest(s): Santo Pirrotta and Reinaldy Hidajat Event Summary: Our membership was offered the rare opportunity to tour the resistance welding department and metallurgical testing laboratory of Lynn Welding, located in Newington, CT. The “Robot” is the creation of Gregg Morisson, long time Lynn…