By lcohnAugust 29, 2024Category: Post Event Report Date of Event: 08/29/2024Location: 4999 E. Bardsley Ave, Tulare, CA 95358Number of Attendees: 47Presenter/Notable Guest(s): Brad Tietjens, Senior NDE Specialist, PG&EEvent Summary: SEE UPLOAD Attendees get together for a group photo. Brad Tietjens (left) is seen receiving a present from Christopher Huff (right). Brad Tietjens is presenting a demonstration on the operation of Magnetic Testing (MT).