Recap: Presentation of the 2024-2025 Section AWS Instructor Award

Date of Event: 12/03/2025

Location: Hanover High School, 401 Moul Avenue, Hanover PA 17331

Number of Attendees: 10-15 attendees.

Presenter/Notable Guest(s): Award presented to Ethan Grove, Hanover PA High School Welding Instructor.
Award presented by Dean Whitmer (Section Treasurer) and Edward Calaman (Section Chairman).

Event Summary: Presentation of the section instructor award was made during the December 2025 Hanover School District Board Meeting.

Dean Whitmer (Section Treasurer), Ethan Grove (Hanover High School Weld Instructor), Edward Calaman (Section Chairman)