Brad Charles Manufacturer’s Representative Mike Charles and Associates Presented demonstration and discussion on 1.5KW laser welding machine with wire feeder.
Brad Charles demonstrated welding mild steel thin gauge metal using a 1.5 laser welding machine with wire feeder. Attendees were able to weld with the equipment and take samples home with them.