Date of Event: 10/29/2025
Location: North Carolina State University
Number of Attendees: 18
Presenter/Notable Guest(s): Ben Labiner – Graduate Research Assistant
Event Summary: Ben Labiner with NC State University gave an awesome presentation on additive manufacturing and how it correlates with the welding industry and materials engineering. After the presentation, we were given a shop tour of NC State Universities Center for Additive Manufacturing & Logistics.