Month: October 2025

Recap: Connecting Welding Innovation: NC State’s Center for Additive Manufacturing & Logistics

Date of Event: 10/29/2025 Location: North Carolina State University Number of Attendees: 18 Presenter/Notable Guest(s): Ben Labiner – Graduate Research Assistant  Event Summary: Ben Labiner with NC State University gave an awesome presentation on additive manufacturing and how it correlates with the welding industry and materials engineering. After the presentation, we were given a shop tour of NC…