Recap: November 2024 AWS Tidewater Section- History of Welding

Date of Event: 11/14/2024 Location: VPCC Workforce Development 600 Butler Farm Road, Hampton VA 23666 Number of Attendees: 52 Presenter/Notable Guest(s): Paul Hebert- Retired Weld Engineer of 38 yrs. with an MS in Welding Engineering “History of Welding” “The Enabling Technologies”. Lynn Showalter- AWS Director at Large and Engineer of the Year. Event Summary: A presentation by…