Date of Event: 02/08/2024
Location: Metro Tech South Bryant Campus 4901 S Bryant Ave. Oklahoma City, OK 73129
Number of Attendees: 25
Event Summary: Six 3 person teams showcased their skills by competing to fabricate & weld a tractor fork. The OKC AWS section donated food and beverages to the participants and judges and promoted the benefits of AWS membership to the students in attendance.