Month: September 2025

Recap: Plant Tour – Alliance Steel, Inc. with an emphasis on robotic welding

Date of Event: 09/18/2025 Location: Alliance Steel, Inc. 3333 S Council Rd. Oklahoma City, OK 73179 Number of Attendees: 45 Presenter/Notable Guest(s): Paul Cribb – Plant Manager for Alliance Steel, Inc. and our tour guide. Event Summary:Paul has 30+ years of fabrication and welding experience and will show us the latest robotic cells for large weldments along…