Recap: Underwater Welding Projects
Date of Event: Oct 7, 2024 Location: Lynnes Welding Training, New Hope MN Number of Attendees: 27 Presenter/Notable Guest(s): Uwe W. Aschemeier Sr. Welding Engineer Subsea Global Solutions, LLC. Uwe Aschemeier is a German born and educated Welding Engineer who has evolved through the metals industry by studying mechanical engineering and welding engineering at various advanced education…