Section #188 Annual Student Welding Contest
Rather than having our typical large gathering for this event the section sent AWS CWIs to each participating school to witness students weld a 3G open root test using SMAW. The CWIs collected the weldments which were brought together to be visually inspected and destructively tested to determine a winner. The top three welders were:…