Date of Event: 10/23/2025
Location: Plantation Inn, 1381 W Tunnel Blvd, Houma, Louisiana
Number of Attendees: 11
Presenter/Notable Guest(s): District 9 Director – Anthony Blakeney
Presenter – Dr. Thomas Shelton – President of Metallurgical & Materials Technologies based on Baton Rouge, LA and officer of the AWS Baton Rouge Section. Presented on Post-weld Heat Treatment Preheat and Interpass Temperatures Metallurgical Considerations
Event Summary: Held a networking social followed by remarks from the Section Chairman, Denis Talbot, and District 9 Director, Anthony Blakeney. A technical session was presented by Dr. Thomas Shelton. Notable attendees included two (2) students from the Fletcher Technical Community College and a guest member from Guyana.