Recap: Hardfacing & repairing a skid steer bucked

Date of Event: 01/03/2024

Location: Lehigh Career & Technical Institute

Number of Attendees: 5

Event Summary: High school students at LCTI were asked to repair cracked welds and complete some hardfacing welds to prolong the life of one of the schools skid steer buckets used in the Heavy Equipment lab. Pictured are Jake Dean (Green coat) and Zach Froshour.

High school students at LCTI were asked to repair cracked welds and complete some hardfacing welds to prolong the life of one of the schools skid steer buckets used in the Heavy Equipment lab. Pictured are Jake Dean (Green coat) and Zach Froshour.
Jake Dean is completing some of the necessary welds to bring the bucket back to life.
Zach Froshour is performing some SMAW welding on the bucket to return it back to the Heavy Equipment lab at Lehigh Career & Technical Insitute