Online Zoom Meeting
ONLINE ZOOM MEETINGChanges in the AWS D1.1 2020 EditionWednesday, October 28th, 2020 Dear Members and Friends, This will be a video conference meeting highlighting the “Major” changes that have occured in the AWS D1.1 Structural Code book, 2020 edition. Format changes – moving to 11 clauses from 9. This change was made to improve clarity…