Recap: Florida West Coast NDE Meeting

Date of Event: 08/21/2025

Location: Southern Technical College 3910 Riga Blvd Tampa FL 33569

Number of Attendees: 80

Presenter/Notable Guest(s): Daryl Peterson-District 5 Director

Event Summary: Daryl Peterson demonstrated Magnetic Particle, Dye Penetrant and Ultrasonic testing of welds.