Recap: Tour of Acceleron, Inc. East Granby, CT

Date of Event: 11/13/2025

Location: 21 Lordship Rd, East Granby, CT

Number of Attendees: 13

Presenter/Notable Guest(s): Vincent Smith, President of Acceleron, Inc. 

Event Summary: Vincent Smith gave a 45 minute presentation on the principles and operations of an electron beam welding system. The presentation was followed by a 45 minute tour of Acceleron’s facilities and showed examples of the types of components they weld. 

Left to Right - Ryan Montano, Vincent Smith, Tim Lucas, Michael Dowd