Date of Event: 03/27/2025
Location: Underground Metal Works 660 W. Kennedy Blvd. Orlando, Fl. 32810
Number of Attendees: 30
Presenter/Notable Guest(s): Jason Becker CWI/CWE Owner of Weldworks Training Center Inc. and Underground Metal Works
Event Summary: Jason Becker did a technical demonstration on Destructive Testing for Performance Qualification. Tests performed were D1.1 Guided Bend Test (Face, Root and Side Bends) D1.1 Macro Etch and Fillet Weld Break Test, D1.3 Sheet Metal Bend Test and a Simulated D1.2 Aluminum Face Bend using a Wraparound Jig.