Date of Event: 05/08/2025
Location: Fall River, Mass
Number of Attendees: Approx. 60+
Event Summary: This was the annual Boston and Central Mass / RI co-section event held at DIMAN RVTHS in Fall River, MA. This event is for networking opportunitys, promoting welding, welding and metal working products, and information on how to become a member of the AWS. This event provided an opportunity to grow professional networks, stay updated on industry advancements and products from various vendors, and winning some great prizes. A custom AWS fire pit crafted by DIMAN students, a custom painted AWS welding helmet, and other welding related items. Also, a chance to earn the title as “best welder of the night” by winning our virtual welding competition on the Lincoln VRTEX welding simulator. This event was attended by 60+ people from various segments of the welding community.