This meeting was a technical meeting where Eric Kuhn and Dennis Johnson, CWI, discussed the different types and importance of bend testing methods: x-ray, macro etching and penetrate testing. They had live demonstrations of different types of bend testing. This meeting was set up for CWIs needing PDH hours.
Fortis technical college had 6 students attend for the knowledge.