November
18,2008 meeting
Speaker was Robert Steinbock
of Superbolt Inc.


 


November
18,2008
Joint Meeting AWS & ASME
Meeting was at
University of Texas @Arlington
Nedderman Hall Room
106
416 Yates St.
Arlington,Texas 76010
The red (A) is where you need to go.
Topic was Gaining the Advantage with Multi-Jackbolt Tensioners
November 13,2007 meeting
November 13,
2007-Distortion,Duplex
Stainless
Firdosh Mehta with Perry
Equip. Mineral Wells
was our speaker. Topic below. Meeting was held at the last minute at the
Golden Corral 1701 N Beltline Rd. Irving, Texas in their private room.
Door Prize Donated by Matheson Tri-Gas
 
Curtis Jenkins with ATI was the lucky winner. Great win Curtis
Firdosh had a great crowd even though
the AWS + Fab Tech Show in Chicago was going on.He brought a show of
their building processes and the engineering of welds and
procedures.Along with his presentation he came bearing jobs with Perry
Equipment. Thanks for coming
 
 



We had a turnout of 45 people.Our food
drive collection was doing very well thanks to the turnouts.
Welcome to the November 13,2006 meeting web
page
Speaker at this meeting was Chuck Meadows with Avesta Welding.Topic was
pickling of stainless steel weldments.He went over the process of
pickling and the different applications it is used on. He explained the
lasting purpose and products of the pickling process. Attendance was
light 18 people showed up. We would recommend Chuck as a speaker to any
section looking for a good topic.
 



Welcome to the November 12,2005 Meeting history
page
Our meeting was a field trip to DFW Airport
and American Airlines
Maintenance Facility. Gywnne Horton was our guide and she really knew
her
stuff. We were lucky to see everything from an L1011 MD to the 777
Beoing. She took us to the spots of the aircraft where welds that were
exposed could be looked at.Engine off the aircraft. Then we took at
look at the maintenance delivery system.
Meeting attendance was 17 people,but it was a Saturday
Thanks again to Gwynne for the tour,it was great.





|